TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Aric parr <[log in to unmask]>
Date:
Wed, 5 Aug 1998 10:14:50 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (72 lines)
I've used them off and on in the past, both for potting and removable
masking.

Problem, the material is hot and has low thermal conductivity. It can
thermal shock parts.

Problem, the material does flow and move in many applications.

Problem, it is difficult to repeatably process in volume without stringing.

It is very inexpensive and easy to use.

I have never had much success in volume production when using it as potting
material. Accuracy, air pockets (from high viscosity and fast setup),
stringing, poor temperature control affecting flow rate, and high
temperature requiring gloves.

ARIC PARR
Sr. Manufacturing Engineer
Eaton Corp
1400 S. Livernois
P. O. Box 5020
Rochester Hills, Mi 48308-5020
[log in to unmask]
248 608 7780
Fax: 248 656 2242
-------------
Original Text
From: C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG, on 8/5/98 10:01 AM:
To: Aric Parr@01635@Lectron_RH,
EatonWHQ@CorpMail@WHQCleveOH[C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG]

Hi Folks,

I have been playing around with some hot-melt adhesives and am somewhat
surprised at how well some of them bond to wire insulation, board materials,
etc.  I really don't know anyone in the government or aerospace biz that is
using this bonding or potting method, and I am wondering 'how come?'
there
may be some very obvious reasons for this, and I'd like to know them. OR,
if
anyone is using hotmelts with success, I would enjoy hearing of it.

Ralph Vaughan
Boeing-Atlanta

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2