>Ben, I have been where you are. Take some Kapton tape and put it over the
>via area that comes in contact with the metal part. Don't rely on solder
>mask to insulate between the two parts as solder mask can be scratched
>easily and flake off. Then you will have a short.
>
>Stephen Corke
>Sr. PWB Designer
>Optical Imaging Systems
>313-207-1274
>
##############################################################