TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Colin Weber <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Colin Weber <[log in to unmask]>
Date:
Mon, 20 Mar 2006 15:32:38 +1100
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Hello Folks,

Could anyone please advise on what realistic long term storage (many years) can
be achieved, and how to achieve it, for components such as integrate circuits?
Any articles or guidelines would be helpful.

We are facing some obsolete component issues and do not have resources to
redesign many boards for incompatible replacements or new devices.

After searching the archives I have ascertained that it seems the hygroscopic
nature of the packages is not a great problem. J-STD-033 should help with
determining storage requirements for this issue. Would it be true to say baking
the components can eliminate any absorbed moisture, even after many years of
long term storage?

A bigger problem appears to be intermetallic growth on the legs, between the
coating (tinning) and the actual leg material.  The intermetallic can grow over
time, eventually causing the legs to lose solderability.  I suspect the growth
rate is temperature dependent and could be slowed by cooling.



Regards,

Colin Weber

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2