TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Thornton White <[log in to unmask]>
Date:
Mon, 14 Mar 2005 09:49:41 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Subject:
From:
Jason Gregory <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<69E4FCAF65C4D511B78D0002A587CB4CC1F6E4@HERMES>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (60 lines)
Answer is either mini-stencil solder paste or flux the areas with paste
flux, then place BGA and reflow. I would go with paste flux (AIM WS300 or
equivalent).

Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)212-0844 cell
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Thornton White
Sent: Monday, March 14, 2005 9:26 AM
To: [log in to unmask]
Subject: [TN]


Hi All.

We have a customer who wants us to place BGA's for them on otherwise
comletely loaded PCB's.
Problem is, the BGA apertures were missed from their stencil.

Is it at all possible to load a BGA straight on to an unpasted (gold finish)
card? What are the quality implications?
Assuming the answer to above is NO, does anyone have UK contacts for BGA
mini-stencils

Any advice would be appreciated.

Thanks in advance.
Thornton

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2