TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Blomberg, Rainer (FL51)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Blomberg, Rainer (FL51)
Date:
Fri, 9 Sep 2005 09:28:40 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (81 lines)
Before cleaning/coating we wear gloves more to protect the operator from
chemicals or things on the "dirty" board. Don't you just hate it when you
pick up a flux-sticky board?  From a contamination stand-point, if the assy
will be cleaned in the near future, handling with bare hands is little risk.
But I've seen some pretty fast corrosion from salty, acidy fingerprints.  We
also wear gloves or finger cots during assy to protect moisture sensitive
components from contamination.  If there are no MS devices we usually just
handle by the edges without gloves, as you probably do.  After cleaning we
wear gloves to protect (maintain) cleanliness or again, handle by the edges.
Wearing gloves can be a real inconvenience (and risky) if not necessary, but
it sure looks good when the customer tours come through.

> Rainer G. Blomberg
> Honeywell -Space Systems Clearwater
> Staff Production Engineer
(727) 539-5534


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Friday, September 09, 2005 11:17 AM
To: [log in to unmask]
Subject: [TN] Clean before cleaning, changed to clean before cooking

Yep,

good considerations on the gloves, thank you.

But what about my original dilemma, wear gloves on assemblies that will be
washed or not? Or, why wearing gloves when you cook, since you are boiling
the ingredients anyways?

And yeah, hockey is good, but football (real football, that you guys call
soccer) is better. Sorry, but I had to mention it, since I started the whole
thing...

Thanks again,
Ioan

> -----Original Message-----
> From: Tempea, Ioan
> Sent: Thursday, September 08, 2005 2:38 PM
> To:   [log in to unmask]
> Subject:      Clean before cleaning
>
> Technos,
>
> the question is whether to wear or not to wear gloves on assemblies that
will be washed. I am fully aware of the solderability problems that can
occur without gloves, so let's stick strictly to the post-wash
contamination.
>
> And in the same key, Doug was talking about not using white gloves that
have chlorines due to bleaching. Which are the gloves to wear?
>
> Thank you,
> Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2