I'm not familiar with the molecular chemistry of polyimides, but your
hypothesis does not seem very likely. At least with epoxies and
polycarbomates, and I assume similarly with other resins, the brominated
flame-retardency compounds are not added particles but form an integral
chemical part of the resin structure, cross-linked into it.
Brian
Prasad Godavarti wrote:
> Dear Friends:
>
> we have an interseting situation: we ordered printed wiring boards that wre
> made from an Isola p96 laminate and the coupons microsections are showing
> what appears to be voids. I understand that these could be brominated
> particles that are added to the polyimide resin to make it fire-retardant.
> How would we verify this? does anyone else have any stories to share on
> what they have seen? I am told this is a finding that may be true only for
> Isola's P96 product that hit the market late last year or early this year?
> need any words of wisdom we can get.
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|