Cal,
If it's an ongoing assembly, I'd get some dedicated selective
wave carriers made to mask the bottom side surface mount. The masking
process you're currently doing shouldn't be causing any of the potential
problems you are concerned about, but does consume a huge amount of
labor that could be directed to something more productive....
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cal Driscoll
Sent: Thursday, March 04, 2004 1:22 PM
To: [log in to unmask]
Subject: [TN] Removable masking/ Double sided reflow
Hello All-
WOW !!! two postings from me in two days...
Here is the case:
We run a double sided reflow process.
We Print, Place, and Reflow the bottom of the boards..
Then
Print, paste, and reflow the top side.
Since the bottom side is mostly discrete and Resistor networks (unlike
the one pictured on Steve's Site) it works well.
For the through hole components we hand insert and solder them.
I just went down to the wave soldering room and found the
operator...........
Covering the bottom side components with removable masking material
(Chemtronics Brand) and sending the boards through wave.
Once Soldered...he removes the masking and all looks well.
Question(s);
1) Is this an acceptable practice?
2) What documentation is available to support or disclaim this?
3) What reliability issues are there due to any thermal mismatch?
4) Any leaching of masking material into the solder join causing poor
joint integrity?
Please advise,
Cal
P.s. Steve be a fountain; not a drain...keep up the excellent work
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|