Dear Lon,
A Eutectic Alloy is best visualised on a phase diagram. It is the mixture of
metals which gives the lowest melting point.
See the Tin/Lead phase diagram attatched with the 183 C (61.9% Sn) eutectic
point marked on it. The triangles to the left and right of this point are
the 'pasty' phases which have already been referred to in other postings.
Hope this helps.
Alan Brewin
Chief Chemist
Concoat Ltd.
2C Albany Park, Frimley Road,
Camberley. Surrey. GU15 2PL. UK.
TEL: +44 (0)1276 691100
FAX: +44 (0)1276 691227
>
>
>Dear friends,
>
>It might seem a stupid question, but what does Eutectic mean when they talk
>about eutectic soldertemperature?
>
>Thanks in advance
>Lon weffers
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>
|
|
|