Lucy..
The UV adhesive that I was referring to, is used primarily for
bonding jumpers to PWB's before conformal coating and after all wave
soldering. For wire tacking, a cure time of 4 to 8 seconds is required
utilizing a UV source with approx .17 watts/cm sq. intensity. I don't
have any info on shear strength, but I would assume that Dymax would
help you with any tech info that you require for their Multi-Cure 911
product. Hope this helps.