Lucy.. The UV adhesive that I was referring to, is used primarily for bonding jumpers to PWB's before conformal coating and after all wave soldering. For wire tacking, a cure time of 4 to 8 seconds is required utilizing a UV source with approx .17 watts/cm sq. intensity. I don't have any info on shear strength, but I would assume that Dymax would help you with any tech info that you require for their Multi-Cure 911 product. Hope this helps. Regards, Bob Vanech Bob Norden Systems *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************