TECHNET Archives

November 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Hollandsworth, Ron" <[log in to unmask]>
Date:
Wed, 10 Nov 1999 13:57:00 -0500
Content-Type:
text/plain; charset="iso-8859-1"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Hollandsworth, Ron" <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Paul:
I would raise my pot temperature.  490 to 500 F is a good temp.  to be at
for the solder pot temperature.

Also check your topside board temperature.  Rule of thumb is 230 F on
topside.  If you have large components on the topside preheating will be
critical.

I looked at your drawing and it looks like you are not getting the heat you
need to solder.  Seeing the pot temp, that low could cause the problem.

Ron Hollandsworth
ITT

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2