TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Vivari, John" <[log in to unmask]>
Date:
Tue, 11 Mar 2003 09:29:19 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
J-STD-001C
7.2.1 Flux Application: When an external flux is used in conjunction
with flux cored solders, the fluxes shall be compatible.
Just a couple of weeks ago Brian Ellis responded to a thread on this
subject. His comments were accurate and important.

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Vivari, John
> Sent: Tuesday, March 11, 2003 9:11 AM
> To: [log in to unmask]
> Subject: [TN] Mixing fluxes - documentation vacuum
>
>
> Dear TechNetters,
>
> A customer of ours came to us with a request for a reference
> to an IPC document or other industry standard that explicitly
> states the hazards of mixing flux types on an assembly.  He
> asked for this because his contract manufacturer built a set
> of boards using a No-clean solder paste and reworked some
> BGAs with a water soluble solder paste.  The contract
> manufacture states that he cannot find a standard "anywhere"
> that says the flux types should not be mixed or that there
> will be any long term reliability issues.  I know this seems
> naive but that is their position.
>
> We have searched our library of specifications, books, and
> industry periodicals and have come up empty except for vague
> statements about having to clean between soldering operations
> for certain classes of product without explaining why and a
> reference in Ning-Cheng Lee's new book cautioning against
> combining incompatible fluxes between reflow and wave
> soldering.  We are well versed in the hazards of mixing our
> own fluxes (never mind others) but have never been asked to
> provide "industry standard documentation" before (as opposed
> to a letter of explanation).
>
> Can anyone point to a reference that we have missed?
>
> Hopefully yours,
>
> John Vivari
> Technical Service Engineer
> EFD Inc.
> [log in to unmask]
> www.efdsolder.com
> Ph: 401-333-3800
> Fx: 401-333-4954
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2