TECHNET Archives

March 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pradeep M <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Pradeep M <[log in to unmask]>
Date:
Mon, 14 Mar 2011 19:01:19 +0530
Content-Type:
text/plain
Parts/Attachments:
text/plain (251 lines)
Hi Richard,

Yes. Only 1 CCA has displayed delamination. Our feeling is that had there
been a problem in pressing, it would definitely have been detected at our
inspection. Also note there is no solder mask. These are quite conspicuous
and we doubt such boards would have slipped through. Even at our customer
end, there is a incoming inspection, where each board is inspected under 40X
magnification in a stereoscope. It has passed through that and also the
assembly. 

Your second guess, we need to check that. The board was electrically
verified in a flying probe tester with a continuity threshold of 5 ohms and
isolation threshold of 99 mega ohms at 100V. We have the BBT report also
available with us. 

Rgds

pradeep



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, March 14, 2011 6:50 PM
To: [log in to unmask]
Subject: Re: [TN] Delam after thermal cycling

It appears the conformal coating was removed around the areas of
delamination. The delaminated areas do not seem to be associated with any
through-hole solder joints, but rather appear in random locations that do
not appear to be related to any other features except that they are located
along inner-layer traces. Because you indicated that this assembly was
"taken up for assembly and manual hand soldering" then I assume no reflow or
wave soldering was performed, only hand soldering. 
I am assuming only one CCA displays these delaminations, but no others in
the lot.
My first guess is that possibly there was a single board fabricated where
the laminate resin was not quite complete, and that small air gaps were left
due to the gap between layers along the traces.
My second guess is that the delamination occurred in these areas because the
traces got hot due to a short or some other overvoltage. Does the CCA
function electrically? If so, then never mind the second theory.

I am still puzzled as to how even small amounts of missing resin could have
delaminated without having gone through some type of thermal cycling hotter
than 60 deg F.

That leaves the possibility that the PWB delaminated during HASL, but went
undetected until after assembly.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, March 14, 2011 7:13 AM
To: [log in to unmask]
Subject: Re: [TN] Delam after thermal cycling

Hi Pradeep,

I have your picture posted here:

http://stevezeva.homestead.com/Delam.jpg

I added the yellow arrows where I think you're showing us the delam. The
larger light areas I'm assuming is conformal coating.

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pradeep M
Sent: Monday, March 14, 2011 5:53 AM
To: [log in to unmask]
Subject: Re: [TN] Delam after thermal cycling

Yes Stephen. Why not? I will send the image to u

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, March 14, 2011 3:09 PM
To: [log in to unmask]
Subject: Re: [TN] Delam after thermal cycling

Pradeep,

Would you like for me to post the photo on my web page for all to see?

Steve

-----Original Message----- 
From: Pradeep M
Sent: Monday, March 14, 2011 5:24 AM
To: [log in to unmask]
Subject: [TN] Delam after thermal cycling

Dear technetters,

We are from a PCB mfg organization. One of our customers has made an
observation on one of the boards that we had supplied to them earlier. This
is a 6 layer card which we had manufactured in July 2007. This board does
not have solder mask and has normal HASL as the surface finish. The customer
had taken this up for manual assembly with hand soldering after some time.
Typically with this customer, the whole assembly usually takes nothing less
than 6-8 months for completion.  They had completed the assembly and had
subjected the assembled board for thermal cycling ( a procedure which they
follow). Thermal cycling is being done at 60 deg C for 2.5 Hrs then at 13
degC for 2.5 Hrs for five cycles.  After this the assembled board has been
coated with conformal coating.  Some more functional tests were conducted
and this card is integrated together with other boards. Then a hot and cold
storage test as part of test and evaluation (T&E) of the package was done.
Storage test (passive ) is at the same extremes but active at 40 deg C. The
customer had opened the package for correcting an anomaly observed, when
they found some 'delamination' on the board.  The customer has sent a
photograph and wants us to respond with our comments. Customer says the
board was looking fine after assembly as well as after the first thermal
cycling.

We are quite surprised on how a delamination can happen at max of 60 deg C.
We do a microsection analysis of every processed panel and also does a
thermal stress as per IPC TM 650 prior to the dispatch. We have asked for
the actual board to ascertain the delamination, but this might take some
time. The conformal coating material removed by peel off manually by the
customer. We had used Nelco 4000-6 170 Tg FR4 material.

Can anybody provide us some inputs. The photograph may be shared directly.

Rgds

Pradeep





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site 
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
----------------------------------------------------- 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2