Subject:
From:
Gabriela <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gabriela <[log in to unmask]>
Date:
Fri, 13 Jan 2012 09:50:58 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (100 lines)
Dear Lum Wei Mei,
If you ask how to be sure of your results, I think that it also depends on
many other factors as circuit built up (internal copper planes, thickness),
height of solder joint (more material, more voltage), Image enhancement
(contrasts, others), and your ability to distinguish the location (which
interface and internal).
I understand your problem, as the results are not easy for interpretation.
You may see voids caused during your reflow process which ARE NOT CAUSED BY
IT.
If you check for voids in BGA balls as received , you may establish
criteria, but on assemblies after reflow it is another story .
In this case, establishing criteria may lead to errors.
Specific for one BGA, you may try to compare your results to a good cross
section on the same balls you checked by X-ray.
Hope this helps,
Gaby 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lum Wee Mei
Sent: ו 13 ינואר 2012 09:29
To: [log in to unmask]
Subject: [TN] BGA X-ray baseline setting

Dear TechNet Buddies,

In IPC-A-600, the standard provides states the inspection magnification
requirement. For external observation : at 1.75x and progress to 40x if
acceptable condition of a suspected defect is not apparent. Such inspection
magnification requirement is not given in IPC-7095 for BGA x-ray. What is
the common industry practice on :

(a)    Tube voltage

(b)   Tube power

(c)    Filter strength

(d)   Averaging

I asked because I worry that I may unintentional set a 'wrong' tube voltage
that could result in the effect known as "Voltage Blooming'. I do not want
to cause false alarm due to my incompetency and result in wrong inspection
judgment on the void size.

Thanks and regards,
~wee mei~


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

__________ Information from ESET NOD32 Antivirus, version of virus signature
database 6790 (20120112) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com


 

__________ Information from ESET NOD32 Antivirus, version of virus signature
database 6790 (20120112) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com
 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2