TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 25 Oct 2002 06:19:31 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
        Solder temp for tinning should be about 500 deg F not C. It should
be used in conjunction with a flux. Remember the hotter the more dross build
up.
        Good Luck
        Ramon


> -----Original Message-----
> From: Hogg, Blair K. [SMTP:[log in to unmask]]
> Sent: Thursday, October 24, 2002 3:38 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Dross on Solder Pot
>
> I turned the pot down yesterday to see what effect it would have. And that
> effect was - the operators turned it back up to (argh) maximum! It
> probably
> is 550C!
>
> It is still as black as ever, and yes the color after wiping off the dross
> could be described as gold.
>
> Now I have to go educate.....
>
> I'm not sure how this is affecting the quality of our products. We
> typically
> tin wires in harness prior to final assembly operations were they are
> soldered to a PCB. And we don't analyze this pot, when the dross gets
> excessive we just replace the solder.
>
> Lots of room for improvement in this process...
>
> Blair
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2