Lon, EUTECTIC refers to an alloy, usually tin/lead, where the melting point
of the alloy is below the melting point of either of the two original
metals. Secondly a eutectic solder alloy has no pasty range, it turns from a
solid to a liquid or liquid to solid without going through a pasty stage as
most other alloys do. There are several eutectic solder alloys i.e..
Sn63/Pb37, Sn 62, Sn96 etc. Refer to J-STD-006 Appendix A. Any solder where
the "Liq" and "Sol" temperatures are the same (indicated by "e" in the "Liq"
column)is said to be a eutectic alloy.
Hope this helps.
Ron Dieselberg
BAE SYSTEMS
Cincinnati Electronics Corp.
-----Original Message-----
From: Lon Weffers [mailto:[log in to unmask]]
Sent: Tuesday, April 25, 2000 15:24
To: [log in to unmask]
Subject: [TN] eutectic
Dear friends,
It might seem a stupid question, but what does Eutectic mean when they talk
about eutectic soldertemperature?
Thanks in advance
Lon weffers
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|