TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 28 Jun 2006 15:54:22 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<008f01c69af8$8d9bc240$6a01a8c0@LjouwertII>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Um........it was Monday??

John

-----Original Message-----
From: Ahne Oosterhof [mailto:[log in to unmask]]
Sent: Wednesday, June 28, 2006 2:20 PM
To: 'TechNet E-Mail Forum'; 'John Burke'
Subject: RE: [TN] Draft exemptions additions

And what was the "technical" background reason for these exemptions? Most
curious about that for numbers 23 and 24.

Ahne.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, 28 June, 2006 11:09
To: [log in to unmask]
Subject: [TN] Draft exemptions additions

Here is the draft of the exemptions list that was approved by the TAC on
their meeting this week. It is draft so presumably not yet written in stone:



John



ANNEX

In the Annex to Directive 2002/95/EC the following points 21 to 27 are
added:

"21. Lead and cadmium in printing inks for the application of enamels on
borosilicate glass.

22. Lead as impurity in RIG (rare earth iron garnet) Faraday rotators used
for fibre optic communications systems.

23. Lead in finishes of fine pitch components other than connectors with a
pitch of 0.65 mm or less with NiFe lead frames and lead in finishes of fine
pitch components other than connectors with a pitch of 0.65 mm or less with
copper lead-frames.

24. Lead in solders for the soldering to machined through hole discoidal and
planar array ceramic multilayer capacitors.

25. Lead oxide in plasma display panels (PDP) and surface conduction
electron emitter displays (SED) used in structural elements; notably in the
front and rear glass dielectric layer, the bus electrode, the black stripe,
the address electrode, the barrier ribs, the seal frit and frit ring as well
as in print pastes.

26. Lead oxide in the glass envelope of Black Light Blue (BLB) lamps.

27. Lead alloys as solder for transducers used in high-powered (designated
to operate for several hours at acoustic power levels of 125 dB SPL and
above) loudspeakers."




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2