Stretching my memory rather a lot but I recall having exactly this
problem which was diagnosed as insufficiently cured resist.
I have no idea why that should be the root cause I just recall it was.
That conclusion was provided to me by a supplier of material to the pcb
manufacturer we were using.
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and
quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
+44 (0)1202 338200
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amarjot Singh
Sent: 21 January 2010 19:59
To: [log in to unmask]
Subject: Re: [TN] Skipping pads in wave solder
Hi Gang:
My customer is having a problem in wave soldering. The board has surface
mount and through hole components on top side and there are some test
points on the bottom side. While passing through wave solder, the holes
are filling nicely but solder is not being coated on some of the test
points. Some test points are in the ground plane (solder mask defined)
and the others is isolated but sorrounded by ground plane. I can cover
those pads using solder iron without any problems.
When performing the similar process at some other assembly house in wave
solder, I noticed the same problem. I played with higher pre-heat
temperatures, slower and faster speed but same result. Any thought on
this issue?
Thanks,
Amarjot
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|