TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Sauer, Steven T." <[log in to unmask]>
Date:
Tue, 21 Oct 2003 06:26:58 -0400
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Sauer, Steven T." <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
Good Morning Karen,
I had the same problem some years back with the cause being identified as
excessive tension on the reel tape during pullback and ESD.  Both were
easily fixed with an adjustment on the feeder to lower the tension and the
placement of an air ionizer within the confines of the placement machine.
Good luck!

Steve Sauer
Sr. Manufacturing Engineer
Northrop Grumman, Xetron

-----Original Message-----
From: Karen Walters

I just want to see if anyone has experienced parts flipping in Pocket
Carrier Tape on Pick and Place Machine and if you could help me identify
some potential root causes.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2