MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Hernefjord Ingemar <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
 Hi,

Anyone who's guru at this? Lids=nickel plated 0.5 mm thick Kovar.
Package= goldplated over nickel plated Kovar.

 We have He leakage problems due to porous and brittle welds. I suspect
that

 a)the 3-4um gold plating on the package is not metallurgically correct,
at least, ought to be much thinner, let's say like flash gold. 

b)too thin nickel on the package, just 1 um, should be 5um or more. 

 c)package shouldn't have electrolytic nickel, but electroless nickel,
because the later has 300 Centigrade lower melting point, and moreover,
is not so brittle (HV300, while EN can be HV1000)

Qs :

what nickel plating do you prefer?

What nickel plate thickness? (Welding, or rather brazing, is
nickel-to-nickel, Kovar should not be involved)

What wheel angle? 9, 12, 15 or what degrees?

Thanks in advance

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2