TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Tempea, Ioan" <[log in to unmask]>
Date:
Thu, 18 Aug 2005 08:52:05 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (AZ75)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Whittaker, Dewey (AZ75)" <[log in to unmask]>
Parts/Attachments:
text/plain (86 lines)
We have done work with these new materials and they have several
advantages over traditional FR4 for High-Rel applications, as well as
being a viable candidate for RoHS compliant requirements. I know some of
you will be concerned that I am staying away from this dicey topic, but
we are not stating phenolic filled or cured systems to classify these
materials, we are calling them non-dicy cured systems. 
This will be reflected in the new slash sheets of IPC-4101/ 99 / 101 /
121 / / 124 and possibly / 126.
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Thursday, August 18, 2005 7:50 AM
To: [log in to unmask]
Subject: Re: [TN] New Resin System

Joe,

a few months ago I had a chat with Dick Woolley of Tyco's PCB division.
He recomended the phenolic filled resin systems as being a must
requirement for a PCB supposed to be ready for  lead-free. Although the
verbage is slightly different, something tells me we are talking about
the same thing.

Maybe he wouldn't mind if you contact him,
[log in to unmask]

Regards,
Ioan

> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Kane, Joseph E (US 
> SSA)
> Sent: Thursday, August 18, 2005 10:27 AM
> To:   [log in to unmask]
> Subject:      [TN] New Resin System
> 
> New Phenolic cured epoxy resin systems are being qualified to 
> IPC-4101/24, 26, and 98 requirements.
> Has anyone tested these new materials?  How do you know which material

> you are really getting (new Phenolic or old DICY cured epoxy resins)?
> 
> Joe Kane
> BAE SYSTEMS
> Johnson City, NY
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET

> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please

> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2