Hi All who have responded to this issue and thank you,
The configuration of pads is for a SIM CARD, the assembly is a Class 2
product, with three pads on opposite sides, L and W 3.3X1.3 mmxmm (130
milsx50mils), pitch is 2.54 mm (100mils). The connections are not the
subject to high currents or voltages, CMOS circuits; the principal function
is for mechanical sustaining. The coating is 1R32A from HumiSeal and the
thickness is about 30 to 50 micro (~ 1mil to 2 mils). After hand soldering
I remove the residues with a hard brush and I repair the coating with a
fresh one by brushing.
Gusti
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|