MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
Dhawan,
See below.

Bev Christian
Nortel

>----------
>From:  Dhawan, Ashok[SMTP:[log in to unmask]]
>Sent:  Saturday, November 01, 1997 10:45 AM
>To:    [log in to unmask]
>Subject:       [TN] FW: ENVIRONMENTAL CONTROL
>
>Post it again for advise on this. I wonder there are no comments on
>this?
>What kind of environmental control being exercised by PCB assembly
houses --for SMT soldering operations?  Can only speak for our plant.
>Whole plant air conditioned, from receving to shipping.  Do you use special
>solder pastes
-less sensitive to slumping/moisture absorption??  No, but I hear that
the Alpha Ultra 78 has very good screen life and I am sure that other
>solder paste producers can also help you out if you ask. More below.Pl do
>comment on this.
>> ----------
>> From:         Dhawan, Ashok
>> Sent:         October 9, 1997 12:41 PM
>> To:   'IPC TechNet'
>> Subject:      ENVIRONMENTAL CONTROL
>>
>> What is kind of environmental control required for a surface mount
>> assembly area.
>> Is pre-reflow soldering operation normally enclosed in restricted
>> ambience of temp and humidity??  Yes, in our company.
>> Is there any IPC standard on facilities requirements on SMT production
>> floor??  Don't know.
>>
>> thanks in advance for all inputs.
>>
>> [log in to unmask]
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2