TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Mike Fenner <[log in to unmask]>
Date:
Tue, 18 Sep 2001 09:36:22 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
From:
Jack Crawford <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (46 lines)
>>> "Mike Fenner" <[log in to unmask]> 09/18/01 05:17AM >>>
Modesty prevents me from claiming to be an expert, but I have some
experience in this area
[Honesty also obliges me to refer you to my company affiliation below],

How can we help?
Best regards

Mike Fenner
Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask] 
W: www.indium.com 
Leadfree: http://Pb-Free.com 

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]]On Behalf Of Jack Crawford
  Sent: Monday, September 17, 2001 6:11 PM
  To: [log in to unmask] 
  Subject: [TN] Solder Preforms ?


  >>> Barry Gallegos [log in to unmask]> 09/17/01 12:02PM >>
  Are there any Solder Preform specialists out there.

  Barry Gallegos
  Process Engineer
  Western Electronics
  1550 South Tech Lane
  Meridian, Idaho 83642
  Phone: 208/955-9771
  Fax: 208/955-9755

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2