TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lum Wee Mei <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lum Wee Mei <[log in to unmask]>
Date:
Fri, 4 Oct 2013 07:36:31 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Glen,
You are correct. It is our regular vendor which we have been using for past many years. The recent some 20 part numbers fabricated by this company has no such observation except for this batch.  

Thanks and Regards,
~wee mei~

"Successful people aren't born that way. They become successful by establishing the habit of doing things unsuccessful people don't like to do. The successful people don't always like these things themselves; they just get on and do them." - William M Thackeray


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Friday, 4 October 2013 1:45 PM
To: [log in to unmask]
Subject: Re: [TN] FW: Grey Matter

Hi Wee Mei 

You could tell me that this is the normal appearance of PWBs from this supplier and I would have to believe you.  However, evidently you have compared it against other boards that you have received from this same vendor and you are seeing a difference.  I recommend asking the vendor to report to you why this lot of boards has a different appearance.  You should have been notified of any changes in the vendor's process.  That vendor runs enough of these boards that EITHER he can tell you why the change in shading on all of his boards OR he should recognize that you have purchased boards for a high reliability application and provide replacements for which there is no concern without needing further analysis first.

I am presuming that this is not a new vendor but one with which you do a regular business.

Glen

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2