Hi Mason! There are a number of different surface reactions which could be
present (silver sulfide, silver chloride, silver oxide, etc.). I use my
SERA test unit with a borate buffer solution to nondestructively analyze
the immersion silver surface to determine who is present. You also could
use Auger spectroscopy too but that would require a destructive analysis.
Dave Hillman
Rockwell Collins
[log in to unmask]
Mason Hu <[log in to unmask]>@IPC.ORG> on 05/30/2001 05:56:25 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Mason Hu <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] Immersion silver boards tarnish
I recently ran a few test assemblies (with immersion Ag finish, of course)
through thermal cycling (for 2nd level reliability). At the end of the
test, some of the non-soldered metal area (EMI contact) got the yellow
tarnish. When probed with a multimeter I measured significant increase in
contact resistance.
I read a lot of comments on the presence of sulfur and chlorine (or their
ionic counterparts) as being the possible root cause. My question is: what
is the chemical reaction(s) here? Are those agents attacking the Ag or the
organic co-deposited with the Ag? Does anybody know what the yellow stuff
is?
Mason Hu
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|