TECHNET Archives

April 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Thu, 19 Apr 2007 09:15:05 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (57 lines)
Well, it is SAC, so it looked ugly to start with, right?  I believe it
will look even uglier--very grainy with lots of protrusions, but none
long enough to bridge the gap between pins.  Depending on how the layers
in your Polyimide board are held together, your laminate may embrittle
drastically.  The ENIG, if done perfectly, will survive, but if there is
any flaw in the nickel process you will see nice black pad failures.

I would be surprised if the solder joints themselves (ignoring the
black pad possibility) did not survive, but obviously the extremely
large grains they would turn into would be even less capable of
accepting some creep than the SAC was originally.

Perhaps if you did this in vacuum or in nitrogen it would look a bit
nicer when it was done cooking.

Wayne Thayer

>>> [log in to unmask] 4/18/2007 2:38:04 pm >>>
Hi all,
 
Just curious, what would you think that a SAC 305 solder joint on a
SOIC
that was made on a ENIG finished polyimide board would do after
spending
140 - 168 hours at 350 F. ?
 
Just wondering is all...
 
-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2