TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Glidden, Kevin" <[log in to unmask]>
Date:
Tue, 14 Aug 2012 14:32:01 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Message-ID:
<000001cd7a4b$1907a640$4b16f2c0$@com>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (41 lines)
I am not sure I can talk to hard or soft gold, and suitability for
soldering. 
But, I can say that it is possible to solder to electroplated gold, which is
different from Immersion Gold finish. 
I think some people say hard gold when they mean electroplated gold. 
There is a brief discussion of this in Coomb's Handbook.
Guy

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Tuesday, August 14, 2012 12:12 PM
To: [log in to unmask]
Subject: [TN] PCB finish: ENIG vs. hard gold

Hi everyone,

We have a PCB supplier who is offering "Hard Gold" as an alternate to ENIG
finish, due to PCB size and processing capabilities.  The application is
Class 3 (mil/aero).  The circuit is thin FR4 and subject to SMT reflow w/
Sn63Pb37 (non RoHS) solder alloy, and moderate flexing in end application.

Can anyone offer info on the differences between the two finishes, and/or
their suitability?  Is there an IPC spec (or specs) that outline "hard
gold"?

Thanks,

Kevin Glidden


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2