TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Newland, Scott" <[log in to unmask]>
Date:
Tue, 1 Apr 2008 14:24:50 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Willis <[log in to unmask]>
Subject:
From:
Bob Willis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (199 lines)
Leaving APEX to fly back to the UK and will send a link to all the
images/x-rays and microsections at the end of the week.

Many thanks

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th May
www.ASKbobwillis.com/faworkshops.pdf
 
 New "Printed Board Inspection & Quality Control" 3 July
www.ASKbobwillis.com/PCBworkshop.pdf 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Newland, Scott
Sent: 01 April 2008 13:03
To: [log in to unmask]
Subject: Re: [TN] Polymer cored solder spheres.

In the US Kyocera has marketed Polymer solder balls

Scott Newland 
Harris GCSD 
321 768 4272 (W)
321 720 1756 (C)
E-Mail [log in to unmask]
 Do you have your CALCE log in?  If not go to:
http://www.calce.umd.edu/accountrequest.html

This information is only intended for the use of the individual or
entity named in this email.  If you are not the intended recipient, you
are hereby notified that any disclosure, copying, distribution, or use
of the contents of this information is strictly prohibited.  If you have
received this email in error, please notify me and delete it
immediately.

-----Original Message-----
From: Bob Willis [mailto:[log in to unmask]] 
Sent: Monday, March 31, 2008 10:18 AM
Subject: Re: Polymer cored solder spheres.

I only know of the supplier in Japan where my parts can from. 

If anyone wants a load of images I took during assembly let me know. I
gave
a load of images, x-rays and sections to Werner so time back, they make
great subjects for x-ray.

Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
 
www.ASKbobwillis.com
 
Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th
May
www.ASKbobwillis.com/faworkshops.pdf
 
 New "Printed Board Inspection & Quality Control" 3 July
www.ASKbobwillis.com/PCBworkshop.pdf 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jenny Drake
Sent: 31 March 2008 09:20
To: [log in to unmask]
Subject: Re: [TN] Polymer cored solder spheres.

Hi Werner,
    I received a couple of responses off the list and will be chasing
them up. Thanks for the extra suggestions. It was your paper in Global
SMT and Packaging that alerted me to the existence of these balls. Early
days yet and I can't go in to details at this stage, but they might help
in the assembly of our product. All depends on cost and availability. 
 
Best regards,  Jenny

________________________________

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: 30 March 2008 23:27
To: [log in to unmask]; Jenny Drake
Subject: Re: [TN] Polymer cored solder spheres.


Hi Jenny,
Nobody responded and I too do not have a European supplier. 
Attached is a column I wrote on this, maybe you have seen it, maybe not.
Possible sources are: [log in to unmask],
[log in to unmask], [log in to unmask],
[log in to unmask], www.solderquik.com,
[log in to unmask], 
Good luck.


Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com



**************
Create a Home Theater Like the Pros. Watch the video on AOL Home.
(http://home.aol.com/diy/home-improvement-eric-stromer?video=15&ncid=aol
hom00030000000001) 

This email contains proprietary information some or all of which may be
confidential, legally privileged and/or otherwise legally exempt from
disclosure and should therefore be considered private. It is for the
intended recipient only. If an addressing or transmission error has
misdirected this e-mail, please notify the author by replying to this
e-mail. If you are not the intended recipient you must not use,
disclose,
distribute, copy, print or rely on this e-mail. When addressed to our
clients any opinions or advice contained in this Internet e-mail are
subject
to the terms of conditions expressed in any of Sarantel's terms of
business.
Incoming communications will be monitored. 

Sarantel Limited
Registered Office: Unit 2, Wendel Point, Wellingborough, NN8 6BA, UK
Registered in England: 3960217            
VAT No.: GB 860 2077 43




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2