Hello Steve,
It is simple. On a PCB select an area where two conductors are running parallel to each
other. Connect a power source through a rheostat. Apply some water drops so as to
cover two tracks. Tap water will be fine. Increase voltage slowly and you should see
migration growth ( depending conductivity of water which you can change by adding
common salt to water). Have fun.
"Stephen R. Gregory" wrote:
> How the heck are yew good ol' boys doin'?
>
> (Spitoooie!!)...'scuse me thar...hadda get rid of my chew, cain't talk with a
> mouthful of terbacky...(hitchin' my bib overalls up)
>
> Anyhoo, a while back, some good ol' boy posted a simple way to actually show
> electromigration (fancy word for us country boys ain't it) in progress...you
> could actually see it happening. Something about using an overhead projector
> and a 9-volt battery...or something like that.
>
> Does anybody remember that? I need some way to graphically show this
> phenomena happening...('nuther fancy word huh?...phenomena...)
>
> YEEEE-HAW!!!
> (that's good ol' boy talk for thanks a lot!)
>
> -Steve "Jethro" Gregory- (GRIN)
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|