TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, William Noel <[log in to unmask]>
Date:
Thu, 1 Mar 2012 08:05:47 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, EIMCNews <[log in to unmask]>
Message-ID:
<001a01ccf7c5$2a837ce0$7f8a76a0$@net>
Subject:
From:
EIMCNews <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (15 lines)
Some are able to plate with better tolerances.  It depends on how the
plating cell is set up for that particular board. What does your board
supplier say?  Admittedly, getting 5 mils anywhere on the surface to achieve
a 1 mil minimum deposit "somewhere" is wasteful of materials, is time
consuming and can compromise the planarity of the surface for subsequent
processes.

You didn't say what problem this overplating is causing.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2