TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ahne Oosterhof <[log in to unmask]>
Date:
Wed, 18 Jun 2014 10:00:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"Joel S. Peiffer" <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (98 lines)
What kind of laser(s) does LPKF use (type, wavelength, power, etc.)

Joel

Joel S. Peiffer
3M Electronic Materials Solutions Division
3M Center, Building 201-1E-17
St. Paul, MN  55144
Tel:  (651) 575-1464
Cell:  (612) 327-1983
[log in to unmask]



From:   Ahne Oosterhof <[log in to unmask]>
To:     <[log in to unmask]>
Date:   06/17/2014 06:26 PM
Subject:        Re: [TN] Laser depanelization
Sent by:        TechNet <[log in to unmask]>



Hi Ed,
Try to get a sample done by LPKF.
12555 SW Leveton Drive, Tualatin, OR.
503-454-4202

Better lasers / much cleaner cut.

Ahne.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Tuesday, June 17, 2014 15:42 PM
To: [log in to unmask]
Subject: [TN] Laser depanelization

Hi all,

One of our aerospace customers is requesting boards depanelized from 
support
frames.

I looked into router, but the conformal coating tends to smear and will be 
a
significant FOD issue later.

We are willing to invest in laser, however, the result is a bit of 
charring
on the edge, not much of a surprise. Unfortunately, this example
http://stevezeva.homestead.com/Capture.JPG was rejected on IPC-A-610-Rev E
Para. 10.7.4 "Solder Mask Coating-Discoloration" "Burned or charred solder
mask material.

In my opinion, this is not within the "spirit of the law" since there are 
no
specific provisions for laser depanelization, only marking.

Anyone know of some way around this?

Ed Popielarski
Engineering Manager

[cid:[log in to unmask]]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0695
                              Cl: 949-581-6601

       "It's one kind of victory to slay a beast, move a mountain, and 
cross
a chasm, but it's another kind altogether to realize that the beast, the
mountain, and the chasm were of your own design."
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.0

11188,0.033023&ctz=420&t=m&z=16&iwloc=A


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2