TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dennis Fritz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 24 Jan 2005 10:57:28 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
Matthew -

I would advise getting a cross section of the silver hole as soon as
possible. The copper in the hole is the current carrying feature, not the final
finish.  I would guess that there is not much copper in these holes, if you can see
the laminate glass bundles visually.  In fact, there is a two sided board
construction, mostly practiced in Asia, that uses no copper.  The silver
containing paste is pulled through the hole with vacuum, and just coats the hole walls.
 This "silver through hole" construction is found mostly in consumer
electronics, that have relatively short use lives.

Denny Fritz
MacDermid

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2