TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, J B Ribeiro <[log in to unmask]>
Date:
Tue, 12 Jul 2011 11:42:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (74 lines)
Hi JB - read this reference paper by John Maxwell - it should be required 
reading for all assembly engineers:

http://www.avx.com/docs/techinfo/cracks.pdf


Dave Hillman
Rockwell Collins
[log in to unmask]



J B Ribeiro <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
07/12/2011 11:23 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
J B Ribeiro <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Capacitor Crack






Hi to all,

We are problems with capacitor crack (0805).
The crack is 45°, close to solder pad and the initiation crack is from 
down to top.

What are the solutions to solver the problem?
Thermal Shock, Pick and Place, Depaneling?

What is the checklist to audit my supplier?

thank you a lot

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2