TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 30 Sep 2009 11:43:47 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (125 lines)
There are different ImAg.  Some of them just added Ag for vision recognition enhancement.  
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Wed Sep 30 11:31:22 2009
Subject: Re: [TN] Immersion Silver for Class 3 Boards

Wayne,

Your first sentence says it all.  People panic about silver migration, which is not really an issue.

I think the paper you are referring to was on creep corrosion.  There have been cases where creep corrosion has been seen on immersion silver boards and that brought about another reason for people to panic. However, the creep corrosion reports I've seen show that creep corrosion occurs when OA flux residue is left on a board and it doesn't matter if the surface finish is immersion silver, immersion tin, or OSP.  Creep corrosion is due to contamination and not to immersion silver.  

Regards,
George
George M. Wenger
Andrew Solutions
Senior Principal FMA/Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 (Office) (732) 309-8964 (cell)
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne - IIW
Sent: Wednesday, September 30, 2009 11:22 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Silver for Class 3 Boards

People panic about silver migration, which is not really an issue.

However, there apparently is a very serious problem that can occur on uncoated boards in high sulfur environments, where somehow the silver acts to catalytically cause the copper to redeposit in random directions.  Doesn't even need a voltage to cause this phenomenon!

A paper on this was brought up to this forum several months back.  If you search the archives on ImAg you should be able to find it.  The growths are nice black dendrites.

Wayne Thayer

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Harner, Chester
Sent: Wednesday, September 30, 2009 11:03 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver for Class 3 Boards

The revised Immersion Silver IPC spec (4553A) indicates that Immersion
Silver is not recommended for Class 3 boards. There is no stated reason.
I have been looking into Immersion Silver for all the same reasons as
everyone else, to replace HASL for flatness etc.  It looked very good
until the Class 3 problem.



Does anyone know why IAg would not be recommended for Class 3 boards?



Chet Harner   Sr. Engineer   Crane Hydro-AirePO Box 7722 Burbank Ca -
91510  818-526-2600 x3557




--------------------------------------------------------------------------------
We value your opinion!  How may we serve you better?
Please click the survey link to tell us how we are doing:
http://www.craneae.com/ContactUs/VoiceofCustomer.aspx
Your feedback is of the utmost importance to us. Thank you for your time.
--------------------------------------------------------------------------------
Crane Aerospace & Electronics Confidentiality Statement:
The information contained in this email message may be privileged and is
confidential information intended only for the use of the recipient, or any
employee or agent responsible to deliver it to the intended recipient. Any
unauthorized use, distribution or copying of this information is strictly prohibited
and may be unlawful. If you have received this communication in error, please notify
the sender immediately and destroy the original message and all attachments from
your electronic files.
--------------------------------------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2