TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Michael McMonagle <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Michael McMonagle <[log in to unmask]>
Date:
Tue, 14 Feb 2006 07:47:13 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
Jon,
        IPC likes the hole not too large to assure good fill and mechanical
integrity. Panasonic likes the hole big enough to drive a truck through to
assure they can insert the part into the hole within the resolution and
repeatability of their insertion system....

Mike McMonagle
Quality Manager
OYO Geospace
7007 Pinemont Drive
Houston, TX 77040
Ph 713-986-8650
Fx 713-986-8725


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jon McDowell
Sent: Monday, February 13, 2006 4:58 PM
To: [log in to unmask]
Subject: [TN] Hole size specs

Technetters

I have a question for you

We are loading a component with a lead diameter of .032 +/-0.002 into a
hole that is .042 +/- 0.003.

On page 20 of IPC-2222 it states in tables 9-4 and 9-5 that with a
tolerance of +/-0.004 the max over sizing in respect to the lead
diameter (on the min side of tolerance) is +/-.023.  Can anyone explain
the reason behind these numbers.

We are using an Panasonic AVKII which call for the hole to be oversized
0.019 from the maximum lead tolerance.

Why would IPC and Panasonic specs not match, this puts us in a difficult
position.


Any help would be appreciated.

Thank You
Jon McDowell
Electronic Controls Co (ECCO)
833 W Diamond St
Boise Id 83705
P 208 395-8025




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2