TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Yuan-chia Joyce Koo <[log in to unmask]>
Date:
Thu, 24 Jul 2014 15:56:34 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (257 lines)
Hi Joyce,

Of course you are right, if customer spec'ed the paste then it is carved in
stone. But maybe they would allow a little leeway with a slight adjustment
in the alloy...

Steve


On Thu, Jul 24, 2014 at 3:33 PM, Yuan-chia Joyce Koo <[log in to unmask]>
wrote:

> Steve, change paste is a major material change,  it might not flight if he
> does not have design authority even to change the pad layout.  he might
> need go up to the food chain (i mean - design... that selected
> material/process and parts).
> imo.
>   jk
> On Jul 24, 2014, at 5:16 PM, Steve Gregory wrote:
>
>  Hi again Steve,
>>
>> I went back and looked for the thread about 2% silver solder paste and
>> it's
>> effect on tomb-stoning. I wanted to find it because I remembered that Dave
>> Hillman gave a very good explanation of why it works, I was able to find
>> it. Below is the thread:
>>
>> Steve Gregory <[log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>>
>>> @[log in to unmask]
>>>
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>>
>> on 09/10/2002 02:16:08 PM
>> Please respond to "TechNet E-Mail Forum." <[log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>>
>>> ;
>>>
>> Please respond to [log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>> Sent by:    TechNet <[log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>>
>>>
>>>  To:    [log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>> cc:
>>
>> Subject:    [TN] 2% Silver solder and tombstoning...
>>
>> Hi All,
>>
>> A while back there was some discussion about 2% silver solder paste and
>> the
>> effect it had reducing tombstones with 0402's.
>>
>> I was skeptical at first, but I decided to try it on a board we build here
>> that quite often has a problem with 0402's tombstoning.
>>
>> To make a long story short, the results were dramatic. Since we've been
>> using the 2% silver paste on this board, tombstones are a very rare
>> exception.
>>
>> I was asked by a new engineer here why I use 2% silver paste to reduce
>> tombstoning, I told him because it really works, I seen it work with my
>> own
>> two eyeballs. But he asked why does that make a difference? That's where
>> I'm kind of stuck...I think I remember that it has something to do with
>> the
>> 2% paste not really being a true eutectic solder, that it's close, but
>> there are slightly different temperatures for solidus and liquidous for
>> that alloy...can anybody educate me again?
>>
>> I did a search and found that Senju had done some studies and found that
>> slight additions of silver and antimony reduced tombstoning to below 10%
>> of
>> that which occured with a 63/37 solder. I think it's either AIM or
>> Multicore
>> also
>> sells what's called a low tombstoning alloy as well.
>>
>> As always, thanks in advance!
>>
>> -Steve Gregory-
>>
>> ************************************************************
>>
>>  Hi Steve! The differences between Sn63 and Sn62 on the tombstone type
>> defects is not voodoo but has a science basis. The Sn63 alloy is a
>> near-eutectic composition with a melting range of slightly above 183C
>> (183C
>> to 188C) - most everyone lists the melting point at 183C but only the true
>> eutectic composition (61.9 Sn) really melts at that temperature. Most of
>> the time this small temperature discrepancy doesn't influence the reflow
>> process. The surface tension of the Sn63 alloy is 490 dyne/cm. The melting
>> range of the Sn62 alloy is 177C-189C (the alloy is not an eutectic
>> composition and therefore doesn't melt a one temperature!). The surface
>> tension of the Sn62 alloy is 376 dyne/cm. And before I get flamed - yes, I
>> know I should be listing the surface tension values at the temperature
>> they
>> were measured by I couldn't get my references quite lined up so please
>> just
>> take them with a grain of salt!  Now all you have to do apply the solder
>> alloy properties to the physical phenomena of tombstoning - tombstoning is
>> hugely influenced by the surface tension of the solder alloys and when
>> melting begins to occur. The Sn62 solder alloy has a slight advantage in
>> that the initial melting temperature is slightly lower and its surface
>> tension is lower meaning it will wet surfaces sooner. It's pretty easy to
>> see why some folks favor the Sn62 alloy over the Sn63 alloy. With all that
>> being said, you should consider one alternative avenue - a change of the
>> component pad geometry also impacts the surface tension forces and could
>> be
>> used as a tombstone fix instead of switching solder alloys!  And as you
>> mentioned - other changes in the solder alloy composition can be used too.
>> I have found that there are two very distinct camps - those who swear by
>> using Sn62 and those who don't - kinda like Doug and I arguing which is
>> better Coke or Mt. Dew!  I know lots of folks who use Sn63 and have no
>> tombstone problems..... and lots of folks who use Sn62 and have no
>> tombstone problems! Just one of those issues in which you have to look at
>> your processes/pwb pad geometries and decide if a either direction fits
>> the
>> way you want to run the solder process. And if you really want to
>> complicate the process throw in the impact of having a 1206 capacitor
>> versus a 0402 capacitor (or a mix of both)! Hope this helps (solder
>> process
>> are just soooo simple!).
>>
>> Dave Hillman
>> Rockwell Collins
>> [log in to unmask]
>> <http://listserv.ipc.org/scripts/wa.exe?LOGON=A3%
>> 3Dind0209%26L%3DTECHNET%26E%3D7bit%26P%3D1153010%26B%3D--
>> part1_cb.280b0562.2ab010a2_boundary%26T%3Dtext%252Fhtml%
>> 3B%2520charset%3DUS-ASCII>
>>
>>
>>
>> On Thu, Jul 24, 2014 at 1:57 PM, Vargas, Stephen M <
>> [log in to unmask]> wrote:
>>
>>  Hello All:
>>>
>>> We are experiencing a high rate of tombstoning on two particular package
>>> styles (0508 and 0612 capacitors) on an assembly here. The rest of the
>>> board solders at a normal defect rate. Here are some of the things we
>>> have
>>> looked at and some aspects of our process:
>>>
>>> I've tried using two different profiles (straight ramp to peak and a
>>> ramp,
>>> soak, spike).
>>> I've moved the parts from our high speed chip shooter to our flexible
>>> placement machine to optimize placement accuracy.
>>> The pad layout (which is not an option for change due to the product
>>> having already been qualified by our customer) is very close to the
>>> manufacturer's recommended layout and the board finish is immersion
>>> silver.
>>> We are printing 1:1, no aperture micro-modifications.
>>> Stencil thickness is 6 mils. I'm concerned about moving to a thicker
>>> stencil due to having 20 mil pitch parts on the board.
>>> Our paste is a low residue / pin probe-able no-clean 63/37 (again not an
>>> option for change).
>>> We also looked at which side of the device is connected to ground,
>>> assuming that this side of the device would heat up more slowly causing a
>>> tombstoning condition pivoting at the non-ground side. But there was no
>>> trend indicating that this was the case.
>>> Solder mask height measured in between the two pads and it was determined
>>> to be at the same height as the pads
>>>
>>> I've attached a link to the datasheet for one of the devices for
>>> reference. I'm wondering if the forces of physics make this part more
>>> susceptible to tombstoning due to the terminations being on the long side
>>> of the device. Any ideas on how we can improve our yields? Thanks.
>>>
>>> http://www.avx.com/docs/Catalogs/licc.pdf
>>>
>>> Regards,
>>> Steve Vargas
>>>
>>> If you don't have time to do it right, when will you have time to do it
>>> over?
>>> John Wooden
>>>
>>> Polaris Contract Mfg Inc
>>> 15 Barnabas Rd
>>> Marion, MA 02738
>>> 774-553-6192
>>> [log in to unmask]<mailto:[log in to unmask]>
>>>
>>> P Please consider the environment before printing this e-mail
>>>
>>>
>>> ______________________________________________________________________
>>> This email has been scanned by the Symantec Email Security.cloud service.
>>> For more information please contact helpdesk at x2960 or
>>> [log in to unmask]
>>> ______________________________________________________________________
>>>
>>>
>> --
>>
>>
>> This email and any attachments are only for use by the intended
>> recipient(s) and may contain legally privileged, confidential, proprietary
>> or otherwise private information. Any unauthorized use, reproduction,
>> dissemination, distribution or other disclosure of the contents of this
>> e-mail or its attachments is strictly prohibited. If you have received
>> this
>> email in error, please notify the sender immediately and delete the
>> original.
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>
>

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2