TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
X-mailer:
Pegasus Mail for Windows (v2.52)
Old-Return-Path:
Date:
Thu, 24 Jul 1997 13:48:30 +0000
Precedence:
list
Comments:
Authenticated sender is <[log in to unmask]>
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
Priority:
normal
TO:
X-Loop:
Return-Path:
<TechNet-request>
X-Mailing-List:
<[log in to unmask]> archive/latest/14275
>From willli Thu Jul 24 12:
35:50 1997
Resent-From:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wrRnZ-000BjyC; Thu, 24 Jul 97 12:35 CDT
Resent-Message-ID:
<"PCbPd1.0.1cK.a9vrp"@ipc>
Subject:
From:
"Robert Welch" <[log in to unmask]>
In-reply-to:
From [log in to unmask] Mon Jul 28 09:
38:32 1997
Organization:
WAYTEC ELECTRONICS CORP
Message-Id:
Parts/Attachments:
text/plain (31 lines)
John, 

Pertaining to the apparent contradictions contained in items #1 & #2, 
as can often happen in this business they are both correct.  Acid 
will indeed help finish crosslinking the polymers if they have not 
completely "kicked over".   However a acid cleaner with a strong 
oxidizer, such as free flouride or chloride ions,  will also help 
undercut and actually remove thin residues prior to surface 
finishing.  Because of this we have a chamber of solder stripper 
prior to our conventional  HASL micro-etch.  We run it only rarely 
when someone or some process up the line goes astray.  Such developer 
problems, excessive hold times, over tack curing, ambient U.V. light 
ETC.  

Robert E. Welch
Process Specialist
Email: [log in to unmask]
Modem: 804-239-9120
Fax:   804-237-3048

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2