TECHNET Archives

February 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 17 Feb 2014 00:24:59 -0500
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Patrick Goodyear <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
Ok industry experts, I’m back to my old stomping grounds for a refuel / 
repair outage.

I have a board that has what appears to be solder reflow or tin plating 
over the top of copper plated edge fingers on the power connections. 
The plated surface was pealed off during cleaning using dust-off 
aerosol.     The pealed pad readily melts under a soldering iron, 
material would be 63-37 solder or pure tin.    It does not appear to be 
silver plating.    The back side of the pealed pieces have a copper 
patina to them, indicating the bonds have failed.

My question is, what is the best way to repair/reflow the fingers?    Do 
they need to be re-plated with copper prior to reflow?   I looked in the 
copy of 7721 we have but can find nothing specific only for replating 
with gold or silver.    This board is used in a HIGH Reliability system.

Pat Goodyear