Gels are an option but it is very easy to exceed J-STD thickness when using
them. Better to seal a connector first with an RTV, if allowed, designed to
be used that thick. We generally mask conservatively and do not coat the
leads at all or, if absolutely required by the customer, go back and touch
them up by hand so they do not get flooded.
Lloyd Duso
Plant Manager
Diamond-MT
(814) 535-3505
www.Diamond-mt.com
On Thu, Feb 8, 2018 at 9:42 AM, Richard Kraszewski <
[log in to unmask]> wrote:
> Agreed and excellent point about the gelled coating.
> Works well if allowed to use.
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and may
> contain information which is privileged, confidential, and/or protected by
> non-disclosure agreements. They are intended solely for the use of the
> named addressee(s). . Any unauthorized use or disclosure may be
> unlawful. If you are not a named addressee, you must not use, disclose,
> retain or reproduce all or any part of the information contained in this
> e-mail or any attachments If you have received this transmission in error,
> please destroy it and notify us immediately by return e-mail or by calling
> + 1 888 208 9005.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Showers
> Sent: Thursday, February 08, 2018 8:11 AM
> To: [log in to unmask]
> Subject: Re: [TN] IPC-CC-830 (Conformal Coat)
>
> I have had some success using Conformal coating gel. One example is 1A33
> Gel. Be advised that it is expensive, nor does not come in user friendly
> packaging.
> More often, if you customer will abide by it, is the application of a
> viscous adhesive such as Hysol 0151. This also can serve as a
> hold-down/part reinforcement.
> If you are NADCAP, please be advised, that until they make a correction,
> the use of Silicon backed masking dots is actually a violation of the