          TO HAWK CHEN
          Hawk, I've seen this problem before and found that the gold 
          bath had a lower gold content which caused more hydrogen 
          gassing and made the plating more inefficient.  This 
          loosened the soldermask at the gold tab interface.  The 
          addition of gold improved the situation.
          
          Another thing which greatly improved all soldermask peel was 
          changing from a chemical preclean to a pumice scrub 
          preclean.  This was especially true when trying to avoid 
          soldermask peel in electroless nickel/immersion gold 
          processing.
          
          Dave Sullivan
          Rockwell Collins, Inc.
          
          [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Solder Mask Peel Off
Author:  [log in to unmask] at ccmgw1
Date:    1/3/97 9:35 PM


Friends:
          
  We encounter a problem with solder mask peel off which is near gold
finger, while after gold plated.
  Is there anybody experience to this problem solution ?
Our solder mask in use is "Tamura" & "Taiyo". Gold plating tank is deep 
type.
          
Thanks and Best Regards,
          
Gloria Electronics, Taiwan
R & D Chief
Hawk Chen
          
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
          

Received: from  by ccmgw1.cacd.rockwell.com (SMTPLINK V2.11)
    ; Fri, 03 Jan 97 21:35:20 cst
Return-Path: <[log in to unmask]>
Received: from stealth.cacd.rockwell.com (stealth) by mailserv with ESMTP
    (1.40.112.8/16.2) id AA073028926; Fri, 3 Jan 1997 21:35:26 -0600
Received: by stealth.cacd.rockwell.com; id VAA08514; Fri, 3 Jan 1997 21:35:39 -0600
Received: from ipc.org(168.113.24.64) by stealth via smap (V3.1.1)
    id xma008509; Fri, 3 Jan 97 21:35:24 -0600
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
     id VAA26399; Fri, 3 Jan 1997 21:26:44 -0800
Resent-Date: Fri, 3 Jan 1997 21:26:44 -0800
Received: by ipc.org (Smail3.1.28.1 #2)
    id m0vgMYk-0000SmC; Fri, 3 Jan 97 21:14 CST
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Message-Id: <[log in to unmask]>
Date: Sat, 04 Jan 1997 23:22:14 +0800
From: Hawk Chen <[log in to unmask]>
Reply-To: [log in to unmask]
Organization: Gloria Electronics Co., LTD.
X-Mailer: Mozilla 3.0Gold (Win95; I)
Mime-Version: 1.0
To: [log in to unmask]
Subject: Solder Mask Peel Off
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit
Resent-Message-Id: <"Gski41.0.ml7.zhSpo"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/8965
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2