TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 16 Mar 2005 18:30:54 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, - Bogert <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
- Bogert <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
March 16, 2005

Does anyone out there know what happens to Ag2.5 (97.5Pb) solder when it is subjected to temperature much above its melting point of 304C?

I posted a capacitor silver braze problem on Technet a couple days ago.  I provided pictures that showed problems with the solder easily flaking off a ceramic to SST braze joint that was made using Ag2.5 solder.

I have been told that if Ag2.5 solder is subjected to temperature > 800C, it can cause solder joint problems like we saw on the capacitor.  Is there any available technical article on this subject?

Does anyone have technical info on corrosion rates for various silver 
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
alloys like Ag 1.5, Ag2.5, Ag 5.5?

ATOM RSS1 RSS2