TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Alderete, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 11 Oct 1999 14:48:55 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (68 lines)
KK-

TEFZEL insulated wire should be more resistant to "cold flow" failure, but I
don't have anything backing this up.

A favorite wire here is MIL-W-22759/33, which uses a modified ETFE
[Ethylene-tetrafluoroethylene], or TEFZEL, insulation.


for more info try

http://www.dupont.com/teflon/chemical/

and contact some wire manufacturers:

http://www.nationalwire.com/index.html

http://www.alphawire.com/index.html

Regards,

Michael Alderete
Aerojet


KK Chin wrote...
------------------------------

Date:    Mon, 11 Oct 1999 11:33:14 -0700
From:    KK Chin <[log in to unmask]>
Subject: Teflon and Tefzel Wire

Dear Technet friends,

We've been using tefzel (a modified teflon) insulated wires in our
transformer
assemblies. Some people are concerned that the teflon's cold-flow property
would
end up in shorts between windings where there are pressure points. My
questions
are:

- Is tefzel better than the unmodified teflon in this respect?
- How is the cold-flow characteristic quantified?
- Where can I find the "cold-flow index" of the materials?

Yours sincerely

K.K. Chin
Artesyn Technologies
Fremont, CA

------------------------------

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2