TECHNET Archives

January 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 24 Jan 2007 17:26:26 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (73 lines)
Hi Jon - the minimum solderability coverage required by the JSTD-002 is 95%
and if a component vendor is not willing to sign up for that requirement,
it means they are not confident that their plating chemistry and/or plating
process can achieve the 95% minimum value. You need to determine if by
accepting a lower minimum value, such as the 90% figure, you will or will
not impact your soldering process workmanship requirements or solder joint
integrity.  Good Luck.

Dave Hillman
JSTD-002 Committee Chair
[log in to unmask]



                                                                           
             Jon Roberts                                                   
             <jroberts@DRS-TEM                                             
             .COM>                                                      To 
             Sent by: TechNet          [log in to unmask]                     
             <[log in to unmask]>                                          cc 
                                                                           
                                                                   Subject 
             01/18/2007 04:12          [TN] MATTE TIN AND SOLDERABLILITY   
             PM                        REQUIREMENTS                        
                                                                           
                                                                           
             Please respond to                                             
              TechNet E-Mail                                               
                   Forum                                                   
             <[log in to unmask]>                                             
             ; Please respond                                              
                    to                                                     
                Jon Roberts                                                
             <jroberts@DRS-TEM                                             
                   .COM>                                                   
                                                                           
                                                                           




Has anyone have Knowledge on solderablity of matte tin finish on
components?
Question came up today from an vendor of the component being purchased
will only guarantee 90% coverage in lieu of J-Std-002 95% coverage and has
requested relief from the J-Std-002 requirement.

Thanks, Jon

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2