TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stewart, Dougal" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 11 Mar 1998 08:51:18 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Why would you want to do this?

Dougal Stewart - Product Development Manager
Viasystems Selkirk Ltd,Scotland TD7 5EJ
Tel: +44 1750 21601
Fax: +44 1750 22513
email: dougal.stewart @ viasystems.co.uk

> -----Original Message-----
> From: Eltek Ltd. - Process Engineering
> [SMTP:[log in to unmask]]
> Sent: Wednesday, March 11, 1998 8:22 AM
> To:   [log in to unmask]
> Subject:      [TN] Innerlayers cleaning
>
> Hi !
> We are considering cleaning of innerlayers by adhesive rollers just
> before
> lay-up . We are applying reduced black oxide , 0.4 mg/sqcm . AOI is
> done
> before black oxide .
> We allready made preliminary test and we had no problems with
> delaminations
> etc . My questions are :
> 1 ) Does anyone performing similar kind of cleaning after black oxide
> ?
> 2 ) What kind of negative effects should be exepcted ?
> Best regards
> Edward Szpruch
> Eltek Ltd - Israel
> Tel  972 3 9395050
> Fax 972 3 9309581
> E-mail :  [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2