We had a serious problem with moisture in our boards. But we use
polyimide with high temp solders. 

You will have to evaluate for your own application.

Paul Stolar
Materials/Reliability Engineer
Manufacturing Reliability Lead Engineer
Baker Atlas
713-625-5376


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Wednesday, April 14, 2004 6:56 AM
To: [log in to unmask]
Subject: Re: [TN] PCB moisture content

Not to my knowledge. There is J-STD-020 and a brief section in HDBK-001.
But
neither set a standard for moisture content.

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Rey Degollado
> Sent: Wednesday, April 14, 2004 7:25 AM
> To: [log in to unmask]
> Subject: [TN] PCB moisture content
>
> Hey Guys,
>
> One of our customers is asking on what is the industry
> standard for pcb moisture content and the method of checking.
> Can somebody please help? Should there be standard reference
> (book, etc) you can recommend.. Better.
>
> Thanks.
>
> Rey Degollado
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2