We had same problem with a batch of ceramic chip capacitors some years
ago. Only way to get rid of the stiff whiskers was reflowing. Maybe
Steve got a place on the wall for my photo, which shows one end of a
chip cap. Pure tin, disaster!
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Gary Camac
Skickat: den 18 november 2005 21:57
Till: [log in to unmask]
Ämne: [TN] Tin whiskers on 0402's in the reel.
Good afternoon,
We have had a problem today with a reel of 0402 resistors where the
placement machine would not pick some of the parts out of the tape
(paper).
A part I examined would not fall out of the pocket when the feeder was
turned upside down. I examine the part sitting in the pocket and it
appeared to be jammed into one corner. After some tapping on the feeder
the
part dislodged. When I examined the part under a microscope, I noticed
a
filament attached to the bottom of the part starting at the corner of
the
electrode. The following part in the tape would, likewise, not fall out
until persuaded. This part fell into my hand and when I examined it
under
the scope I could see a filament lying beside it in my palm.
These parts are a 2002 date code. Tin whisker? Anyone seen this
before?
I took the reel on components to our environmental test lab, bolted it
to
the sinusoidal vibration table and shook for about a minute. We then
reinstalled the reel on the placement machine and the picking problem
went
away. Interesting stuff for a Friday afternoon.
Gary Camac
Senior Mfg. Eng.
Dickey-john Corp.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|