TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Kelly <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Wed, 2 May 2007 11:45:17 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
Good Morning,

I need some opinions on a flexible soldermask problem but I need to post the
pictures to Steve's web site.

The picture will show the flexible soldermask has separated apart
(separation is approx .0002 wide). In our opinion it is not a crack or a
conventional crack. The separation only occurs on top of the acrylic
adhesive in the frame which surrounds the part which is free of copper. It
never occurs on top of the copper. The separation occurs in approx. 10-15%
of the parts we are building in the same batch built at the same time. The
separation is there after "tack cure" and does not get worse after full cure
or HASL.  When we solder float the part without baking the separation does
not propagate - get any larger or do anything. The IPC-SM-840 really does
not address flexible soldermasks well so my questions are 1)  any thoughts
on what is causing this 2) reliability issues - part goes into a super
computer which will be in a controlled environment - application is not
dynamic. 

Thanks in advance.

Regards Steve Kelly


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2