Hello Henry,
I came across the same problem. A temporary solution for me was to apply a
good layer of peelable solder mask over the underside vias. This reduced my
temperatures under the bga by 20C.
A permanent fix, in my case, was to go double sided reflow with pin in hole
reflow where appropriate.
Hope this helps,
Regards
Eric Dawson
> -----Original Message-----
> From: Henry Rekers [SMTP:[log in to unmask]]
> Sent: Wednesday, June 26, 2002 3:08 PM
> To: [log in to unmask]
> Subject: [TN] Reflow on Wave.
>
> Does anybody have any suggestions on avoiding reflow of a 357 ball bga on
> the wave? I'm dealing with a 6 layer board and I've kept the preheat as
> low
> as possible. Kapton tape doesn't seem to help. Has anybody tried any
> custom manufactured sheilding?
>
> Thanks.
>
> Henry J. Rekers
> Manufacturing Engineer.
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|