Hi Paul,
A chelating type resin would be the best for heavy metals removal, but it is very expensive. Control of the pH level is important for selectivity, so be sure to request selectivity data at different pH levels. If you need more information on this part let me know and I will share my experiences. We are a small circuit board shop here in the Chicago area and we have a two-train ion exchange system plus a two-column deionizing system for making DI water from city water.
Two manufacturers whose resins I have used are:
Rohm and Haas
5000 Richmond St.
Philadelphia, PA 19137
215-537-4060
Pureolite Corp.
150 Monument Road
Bala Cynwyd, PA 19004
800-343-1500
Pureolite resin tends to be less expensive but seems to work equally well. I am currently using the Pureolite resin in all my columns.
Feel free to contact me if you have any questions.
Sincerely,
Michael S. Owens
Manager, Safety & Environmental Compliance
Poly Circuits, Inc.
216 Evergreen St.
Bensenville, Illinois 60106
630-860-3560 x157
[log in to unmask]
################################################################
ComplianceNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE ComplianceNet <your full name>
To unsubscribe: SIGNOFF ComplianceNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|